Title of Invention

A SANITARY NAPKIN ADAPTED TO BE WORN IN A CROTCH PORTION OF AN UNDERGARMENT

Abstract A sanitary napkin adapted to be worn in a crotch portion of an undergarment, said sanitary napkin comprising: a) a fluid-pervious cover layer (42); b) an absorbent system (44) under said cover layer (42) said absorbent system (44) having a central width of at least 64 mm; c) a liquid-impervious barrier layer (50) under said absorbent system(44); d) said sanitary napkin being characterised by a thickness less than about 5mm; e) said sanitary napkin being characterised by a flexural resistance of not less than about 400 g; f) said sanitary napkin having a main body (20) with a longitudinal axis (34) and two opposite longitudinal side areas (30,32) said sanitary napkin including a preferential bending line extending obliquely in relation to said longitudinal axis on said main body, said preferential bending line extending from one longitudinal side area of the sanitary napkin to an opposite longitudinal side area, crossing the longitudinal axis of the sanitary napkin.
Full Text

THIN SANITARY NAPKIN CAPABLE OF CONTROLLED DEFORMATION WHEN IN USE
FIELD OF THE INVENTION

The present invention relates generally to the art of fluid absorption and
more particularly to a disposable sanitary napkin that is thin, highly absorbent
and is capable of controlled deformation when in use.
BACKGROUND OF THE INVENTION
One element that contributes to the performance of a sanitary napkin
is the way the napkin withstands deformation when in use. It has been
observed that the thighs of an individual exert lateral forces on a sanitary
napkin when the article is positioned for use on the undergarment. This
results in bunching of the sanitary napkin, affecting the efficiency of the
article's ability to collect bodily fluids since there is a concomitant reduction
in the article's surface area. This observation is especially true for thin
sanitary napkins that are highly flexible.
One approach to minimising this problem is to make the sanitary
napkin stiffer in order that it may better withstand the effects of lateral
compression. This approach may, however, have an adverse effect on the
comfort potential of the sanitary napkin because the added stiffness affects
the movement of the napkin in all directions, making it more difficult for the
napkin to conform to the natural shape of the wearer's body.

Against this background, it can be seen that there exists a need to
provide a sanitary napkin that is comfortable and yet reduces the likelihood
of bunching when in use, leading to an overall increase in its efficiency for
collecting bodily fluids.
SUMMARY OF THE INVENTION
It has been discovered that when a sanitary napkin is provided with at
least one preferential bending zone in its absorbent system, the effect is to
promote the folding of the absorbent system along this preferential zone and
to promote a certain three-dimensional deformation profile in the napkin in
response to lateral compression exerted by the thighs of the wearer. The
sanitary napkin has a flexural resistance that is not less than about 400 g.
This feature provides a sanitary napkin that is sufficiently stiff, so as to be
stable enough and thus allow the sanitary napkin to fold in a predictable
manner and avoid the likelihood of bunching when subjected to lateral
compression.
In one aspect of the invention, the absorbent system of the sanitary
napkin includes two preferential bending zones extending longitudinally near
the side edges of the napkin and a central preferential bending zone
extending longitudinally in the central portion of the absorbent system.
in use, the sanitary napkin assumes a three-dimensional deformation profile
that resembles the letter W, in response to the lateral forces exerted by the
thighs of the wearer. in a specific example of implementation, the sanitary
napkin includes a plurality of preferential bending lines that extend obliquely
relative to the longitudinal axis of the napkin and intersect each other. The
preferential bending lines cross one another and form an array of crossing

points. The crossing points are located along the longitudinal axis of the
sanitary napkin and structurally weaken the sanitary napkin at that location
allowing the sanitary napkin to fold preferentially along its longitudinal axis.
The array of crossing points forms the central preferential bending zone.
The preferential bending zone under any one of the aspects of the
invention presented above may be realised by means of any one of the
following: perforations, slits, cuts and embossing, as well as any other
processes known to a person skilled in the art that has the effect of locally
weakening the material in which the preferential bending zone is to be
created.
Other aspects and features of the present invention will become
apparent in those ordinarily skilled in the art upon review of the following
description of specific embodiments of the invention in conjunction with the
accompanying drawings.
DESCRIPTION OF THE DRAWINGS
v..
Figure 1 is a top elevational view of a sanitary napkin in accordance
with the present invention, the cover layer of the sanitary napkin being partly
removed to show the absorbent system.
Figure 2 is a perspective view of the sanitary napkin of Figure 1,
depicted in a position attained when the sanitary napkin is placed in the
undergarment of a wearer.

Figure 3 is a bottom plan view of the sanitary napkin shown in Figure
1.
Figure 4 is a cross-sectional view taken along the longitudinal
centerline of the sanitary napkin shown in Figure 3.
Figure 5 is a schematic illustration of means for air-laying absorbent
material for making an example of an absorbent layer of the absorbent
system of the sanitary napkin according to the invention, using four air-laying
heads followed by means for compacting the air-laid material.
Figures 6(a) and 6(b) show three and four stratum embodiments,
respectively, of an absorbent layer that can be used in the construction of
the absorbent system of the sanitary napkin in accordance with the
invention.
Figures 7 to 10 are cross-sectional views of an absorbent layer of the
absorbent system of the sanitary napkin in accordance with the invention
featuring different patterns of preferential bending zones allowing the
sanitary napkin to fold in use according to a certain three-dimensional
pattern.
Figure 11 is a cross-sectional view of the sanitary napkin shown in
Figure 1, depicting the napkin folded according to a W pattern.
Figure 12 is a cross-sectional view of the sanitary napkin shown in
Figure 1, depicting the napkin folded according to a "M" pattern.

Figure 13 is a cross-sectional view of the sanitary napkin shown in
Figure 1, depicting the napkin folded according to a "V' pattern.
Figure 14 is a cross-sectional view of the sanitary napkin shown in
Figure 1, depicting the napkin folded according to an inverted "V" pattern.
DETAILED DESCRIPTION
Referring to Figures 1 and 2, there is shown an embodiment of the
present invention, a feminine sanitary napkin 20.
The sanitary napkin 20 has a main body 22 with a first transverse side
26 defining a front portion thereof and a second transverse side 28 defining a
rear portion thereof. Each of these sides is arcuate or of any other suitable
shage.The main body also has two longitudinal sides, namely a longitudinal
side 30 and a longitudinal side 32. The sanitary napkin 20 has a thickness not
exceeding about 4 mm. Preferably, the thickness is less than 3.5 mm, more
preferably less than 2 mm, and most preferably, it is of about 2.8 mm.
The sanitary napkin 20 has a longitudinal centerline 34 that is an
imaginary line bisecting the sanitary napkin 20 in two identical halves.
In the embodiments shown in the drawings the sanitary napkin is
provided with a pair of side flaps 38, 40. The flaps 38, 40 project laterally
outward from each of the longitudinal sides 30, 32 and are adapted to be
folded over a crotch portion of a wearer's undergarment. The flaps 38, 40
are in the shape of an isosceles trapezoid with the top adjoining the
longitudinal side and the base at the distal end.

The main body 22 also has an imaginary transverse centerline 36
perpendicular to the longitudinal centeriine 34 and simultaneously bisecting the
flaps 38,40.
As depicted in Figure 4, the main body 22 is of a laminate construction
and preferably comprises a fluid-permeable cover layer 42, an absorbent
system 44, and a fluid-impervious barrier layer 50. The absorbent system has
preferably two components, namely a first absorbent layer 46 (commonly
known as "transfer layer") and a second absorbent layer 48 (commonly known
as "absorbent core"). Alternatively, a single layer, namely the second
absorbent layer 48, can form the absorbent system 44. Each of these layers is
described in hereinbelow.
Main Body-Cover Layer
The cover layer 42 may be a relatively low density, bulky, high-loft non-
woven web material. The cover layer 42 may be composed of only one type of
fiber, such as polyester or polypropylene or it may be composed of bi-
component or conjugate fibers having a low melting point component and a
high melting point component. The fibers may be selected from a variety of
natural and synthetic materials such as nylon, polyester, rayon (in combination
with other fibers), cotton, acrylic fiber and the like and combinations thereof. An
example is the non-woven cover layer of sanitary napkins sold by Johnson &
Johnson Inc. of Montreal, Canada under the trademark Stayfree Ultra-Thin
Cottony Dry Cover.

Bi-component fibers may be made up of a polyester core and a
polyethylene sheath. The use of appropriate bi-component materials results
in a fusible non-woven fabric. Examples of such fusible fabrics are described in
U.S. Patent 4,555,446 issued November 50,1985 to Mays. Using a fusible
fabric increases the ease with which the cover layer may be mounted to the
adjacent first absorbent layer and/or to the barrier layer.
The cover layer 42 preferably has a relatively high degree of
wettability, although the individual fibers comprising the cover may not be
particularly hydrophilic. The cover material should also contain a great
number of relatively large pores. This is because the cover layer 42 is
intended to take-up body fluid rapidly and transport it away from the body
and the point of deposition. Advantageously, the fibers which make up the
cover layer 42 should not lose their physical properties when they are
wetted, in other words they should not collapse or lose their resiliency when
subjected to water or body fluid. The cover layer 42 may be treated to allow
fluid to pass through it readily. The cover layer 42 also functions to transfer
the fluid quickly to the other layers of the absorbent system 44. Thus, the
cover layer 42 is advantageously wettable, hydrophilic and porous. When
composed of synthetic hydrophobic fibers such as polypropylene or bi-
component fibers, the cover layer 42 may be treated with a surfactant to
impart the desired degree of wettability.
Alternatively, the cover layer 42 can also be made of polymer film
having large pores. Because of such high porosity, the film accomplishes the
function of quickly transferring body fluid to the inner layers of the absorbent
system. Apertured co-extruded films such as described in U.S. Patent

4,690,679 and available on sanitary napkins sold by Johnson & Johnson Inc.
of Montreal, Canada could be useful as cover layers in the present invention.
The cover layer 42 may be embossed to the remainder of the
absorbent system 44 in order to aid in promoting fluid transport by fusing the
cover to the next layer. Such fusion may be effected locally, at a plurality of
sites or over the entire contact surface of cover layer 42 with absorbent
system 44. Alternatively, the cover layer 42 may be attached to the
absorbent system 44 by other means such as by adhesive.
Main Body - Absorbent System -First Absorbent Layer
Adjacent to the cover layer 42 on its inner side and bonded to the
cover layer 42 is a first absorbent layer 46 that forms part of the absorbent
system 44. The first absorbent layer 46 provides the means of receiving
body fluid from the cover layer 42 and holding it until an underlying second
absorbent layer has an opportunity to absorb the fluid.
The first absorbent layer 46 is, preferably, more dense than and has a
larger proportion of smaller pores than the cover layer 42. These attributes
allow the first absorbent layer 46 to contain body fluid and hold it away from
the outer side of the cover layer 42, thereby preventing the fluid from re-
wetting the cover layer 42 and its surface. However, the first absorbent layer
46 is, preferably, not so dense as to prevent the passage of the fluid through
the layer 46 into the underlying second absorbent layer 48. These types of
absorbent layers are commonly known as fluid transfer layers or acquisition
layers.

The first absorbent layer 46 may be composed of fibrous materials,
such as wood pulp, polyester, rayon, flexible foam, or the like, or
combinations thereof. The first absorbent layer 46 may also comprise
thermoplastic fibers for the purpose of stabilizing the layer and maintaining
its structural integrity. The first absorbent layer 46 may be treated with
surfactant on one or both sides in order to increase its wettability, although
generally the first absorbent layer 46 is relatively hydrophilic and may not
require treatment. The first absorbent layer 46 is preferably bonded on both
sides to the adjacent layers, i.e. the cover layer 42 and an underlying second
absorbent layer 48. An example of a suitable first absorbent layer is a
through air bonded pulp sold by BUCKEYE of Memphis Tennessee under
the designation VIZORB 3008.
Main Body - Absorbent System—Second Absorbent Layer
Immediately adjacent to and bonded to the first absorbent layer 46 is
the second absorbent layer 48.
In one embodiment, the absorbent system has a first absorbent layer
46 having a central width of at least about 60 mm. The absorbent system
further has a second absorbent layer 48 having a central width that is about
the same width as the first absorbent layer 46. in a preferred embodiment,
the central width of both the first absorbent layer 46 and the second
absorbent layer 48 is greater than about 60 mm. in another embodiment,
the first absorbent layer 46 has a central width that exceeds the central width
of the second absorbent layer 48. The term "central width" refers to a
specific area of a layer, such as an absorbent layer determinable as follows.
A reference point on the sample layer that is disposed beneath the center of

the vaginal orifice, when worn, is located. A plane parallel to the transverse
centerline 36 and 3.75 centimeters forward from the reference point in the
direction of the wearer's mons pubis is located. Another plane parallel to the
lateral centerline 36 and 5.0 centimeters rearward from the reference point in
the direction of the wearer's buttocks is also located. The greatest flat-out,
uncompressed, unmanipulated, lateral width of the sample layer between the
two planes is the absorbent width of the sample layer.
The central width of the absorbent system, when the absorbent
system includes a plurality of absorbent layers is the central width of the
layer of the absorbent system that has the largest central width. in a
specific example, the central width of the absorbent system exceeds 60 mm
and preferably exceeds 64 mm.
In one embodiment, the second absorbent layer 48 is a blend or
mixture of cellulosic fibers and superabsorbent disposed in and amongst
fibers of that pulp.
In a specific example, the second absorbent layer 48 is a material
containing from about 40 weight percent to about 95 weight percent
cellulosic fibers; and from about 5 weight percent to about 60 weight percent
SAP (superabsorbent polymers). The material has a water content of less
than about 10 weight percent. As used herein, the phrase "weight percent"
means weight of substance per weight of final material. By way of example,
10 weight percent SAP means 10 g/m2 SAP per 100g/m2 basis weight of
the material.

Cellulosic fibers that can be used in the second absorbent layer 48
are well known in the art and include wood pulp, cotton, flax and peat moss.
Wood pulp is preferred. Pulps can be obtained from mechanical or chemi-
mechanical, sulfite, kraft, pulping reject materials, organic solvent pulps, etc.
Both softwood and hardwood species are useful. Softwood pulps are
preferred. It is not necessary to treat cellulosic fibers with chemical
debonding agents, cross-linking agents and the like for use in the present
material.
The second absorbent layer 48 can contain any superabsorbent
polymer (SAP), which SAPs are well known in the art. For the purposes of
the present invention, the term "superabsorbent polymer" (or "SAP") refers to
materials which are capable of absorbing and retaining at least about 10
times their weight in body fluids under a 0.5 psi pressure. The
superabsorbent polymer particles of the invention may be inorganic or
organic crosslinked hydrophilic polymers, such as polyvinyl alcohols,
polyethylene oxides, crosslinked starches, guar gum, xanthan gum, and the
like. The particles may be in the form of a powder, grains, granules, or fibers.
Preferred superabsorbent polymer particles for use in the present invention
are crosslinked polyacrylates, such as the product offered by Sumitomo
Seika Chemicals Co., Ltd. Of Osaka, Japan, under the designation of SA60N
Type II*, and the product offered by Chemdal International, Inc. of Palatine,
Illinois, under the designation of 2100A*.
In a specific example the second absorbent layer 48 is a material
containing from about 50 to about 95 weight percent cellulosic fibers and,
more specifically from about 60 to about 80 weight percent cellulosic fibers.
Such a material may contain from about 5 to about 60 weight percent SAP,

preferably from about 20 to about 55 weight percent SAP, even more
preferably from about 30 to about 45 weight percent SAP, and most
preferably about 40 weight percent SAP.
The second absorbent layer 48 can be manufactured by using air-
laying means well known in the art (See Figure 5). in accordance with Figure
5, cellulosic fibers (e.g., pulp) are processed using a hammer mill to
individualize the fibers. The individualized fibers are blended with SAP
granules in a blending system 1 and pneumatically conveyed into a series of
forming heads 2. The blending and distribution of fibers and SAP granules
can be controlled separately for each forming head. Controlled air circulation
and winged agitators in each chamber produce uniform mixture and
distribution of pulp and SAP. The SAP can be thoroughly and
homogeneously blended throughout the material or contained only in
specific strata by distributing it to selected forming heads. Fibers (and SAP)
from each forming chamber are deposited by vacuum onto a forming wire 3
thus forming a layered absorbent web. The web is subsequently compressed
using calenders 4 to achieve desirable density. The densified web is wound
into a roll 5 using conventional winding equipment. The forming wire 3 can
be covered with tissue paper to reduce the loss of material. The tissue paper
layer can be removed prior to calendering or incorporated into the formed
material. in a possible variant, the first absorbent layer 46 can be formed
integrally with the second absorbent layer 48 to provide a unitized absorbent
system 44. This can be achieved by providing the apparatus depicted in
Figure 5 with an additional forming head (not shown in the drawings) to
deposit on the second absorbent layer 48, by air laying and prior to
calendering, a layer of material to form the first absorbent layer 46.

The second absorbent layer 48 of the present invention is of high
density and in a specific example has a density of greater than about 0.25
g/cc. Preferably, the second absorbent layer 48 may have a density in the
range of from about 0.30 g/cc to about 0.50 g/cc. More preferably, the
density is from about 0.30 g/cc to about 0.45 g/cc and, even more preferably
from about 0.30 g/cc to about 0.40 g/cc.
Air-laid absorbents are typically produced with a low density. To
achieve higher density levels, such as the examples of the second absorbent
layer 48 given above, the air-laid material is compacted using calenders as
shown in Figure 5. Compaction is accomplished using means well known in
the art. Typically such compaction is carried out at a temperature of about
100 degrees C and a load of about 130 Newtons per millimeter. The upper
compaction roll is typically made of steel while the lower compaction roll is a
flexroll having a hardness of about 85 SH D. It is preferred that both the
upper and lower compaction rolls be smooth, although the upper roll can be
engraved.
In one embodiment the second absorbent layer 48 has a ratio of
Gurley stiffness, measured in milligrams (mg) to density, measured in grams
per cubic centimeter (g/cc), of less than about 3700. in a specific example,
that ratio of Gurley stiffness to density is less than about 3200 and, more
specifically, less than about 3000.
Gurley stiffness is one of many indices of softness. Gurley stiffness
measures the bendability or flexibility of absorbent materials. The lower the
Gurley stiffness value, the more flexible the material. The Gurley stiffness
values are measured using a Gurley Stiffness Tester (Model No. 4171E),

manufactured by Gurley Precision Instruments of Troy, N.Y. The instrument
measures the externally applied moment required to produce a given
deflection of a test strip of specific dimensions fixed at one end and having a
concentrated load applied to the other end. The results are obtained in
"Gurley Stiffness" values in units of milligrams.
The second absorbent layer 48 is strong in light of its softness. Pad
integrity is a well-known measurement of absorbent material strength. in a
specific embodiment the second absorbent layer 48 demonstrates strength
(high pad integrity) over a wide range of densities. in a specific example the
second absorbent layer 48 has a pad integrity, measured in Newtons (N), to
density (g/cc) ratio of greater than about 25.0. in a more specific example,
that ratio is greater than about 30.0 and, could even be greater than about
35.0. The pad integrity is a test performed on an Instron Universal Testing
Machine. Essentially, the test measures the load required to pierce through
the test sample, as described in the PFI Method of 1981. A test sample
having dimensions of 50 mm by 50 mm is clamped on the Instron with a
suitable fastening device. A 20 mm diameter piston traveling at the rate of 50
mm/min punctures the stationary sample. The force required to puncture the
sample is measured in Newtons (N).
The second absorbent layer 48 can be prepared over a wide range of
basis weights. The second absorbent layer 48 can have a basis weight in the
range of from about 100 g/m2to about 700 g/m2. in a specific example, the
basis weight ranges from about 150 g/m2 to about 350 g/m2 . Preferably
the basis weight ranges from about 200 g/m2 to about 300 g/m2 and, more
preferably, to about 250 g/m2.

The second absorbent layer 48 can be formed as three or four lamina
or strata. Those strata include a bottom layer, one or two middle layers and a
top layer. Specific examples of three and four layer material are set forth
below. The SAP can be included in any or all of the layers. The
concentration (weight percent) of SAP in each layer can vary as can the
nature of the particular SAP.
An interesting characteristic of the second absorbent layer 48 is its
ability to retain SAP when subjected to mechanical stress. The second
absorbent layer 48 retained over 85 percent by weight of its SAP content
when subjected to 10 minutes of rigorous shaking. Specifically, a material of
this invention retains over 90 percent, more specifically over 95 percent and,
even more specifically over 99 percent of its SAP under these mechanical
stresses. The percent of SAP retained was determined by shaking the
material in a Ro-Tap Sieve Shaker manufactured by W. S. Tyler Co.,
Cleveland Ohio. More specifically the sample is placed in a 28-mesh (Tyler
series) sieve. Additional sieves of 35-mesh and 150-mesh were attached to
the first sieve forming a column of increasingly fine sieves. The column of
sieves was capped on either end to prevent the loss of fiber and/or SAP. The
sieve column was placed in the shaker and agitated for 10 minutes. The
amount of SAP granules shaken loose from the sample, "free SAP", was
determined by combining the residue contained in each of the sieves and
separating the cellulosic fiber from the SAP.
Even where prepared as from multiple layers, the final thickness of
the formed second absorbent layer 48 is low. The thickness can vary from
about 0.5 mm to about 2.5 mm. in a specific example, the thickness is from

about 1.0 mm to about 2.0 mm and, even more specifically from about 1.25
mm to about 1.75 mm.
One embodiment of the second absorbent layer 48 particularly well
suited for use in the sanitary napkin 20 is depicted in Figure 6. Such second
absorbent layer 48 has a basis weight of from about 200 g/m2 to about 350
g/m2 and a density between about 0.3 g/cc and 0.5 g/cc. in a specific
example, the density is from about 0.3 g/cc to about 0.45 g/cc and, more
specifically about 0.3 g/cc to about 0.4 g/cc.
The second absorbent layer 48 depicted in Figure 6(a) is air-laid as
three strata: a bottom layer of pulp (without superabsorbent) with a basis
weight of about 25 g/m2; a middle layer with a basis weight of about 150
g/m2 and which contains from about 10 to about 30 g/m2 superabsorbent
and from about 120 g/m2 to about 140 g m2 pulp; and a top layer of pulp
(without superabsorbent) with a basis weight of about 25 g/m2. Relative to
the total basis weight of the second absorbent layer 48, the level of
superabsorbent ranges from about 5 to about 15 weight percent (g/m2 of
superabsorbent per g/m2 material). in a specific example, the level of
superabsorbent is from about 7.5 weight percent to about 12.5 weight
percent of the material. More specifically, the material contains about 10
weight percent of superabsorbent. Thus, the middle layer of the material
could contain from about 15 g/m2 to about 25 g/m2 superabsorbent and
from about 125 g/m2 to about 135 g/m2 pulp and, more specifically about 20
g/m2 superabsorbent and about 130 g/m2 pulp. The middle layer containing
pulp and superabsorbent can be laid down as a homogeneous blend or as a
heterogeneous blend wherein the level of superabsorbent varies with
proximity to the bottom layer.

In another embodiment depicted in Figure 6(b), the second absorbent
layer 48 is air-laid as four strata. in this embodiment, the middle layer
referred to above is replaced with two middle layers: a first middle layer
adjacent the top layer and a second middle layer adjacent the bottom layer.
Each of the first and second middle layers independently comprises from
about 10 to about 30 g/m2 superabsorbent and from about 40 g m2 to about
65 g/ m2 pulp. When it is desired to keep absorbed fluid away from the cover
layer 42 the amount of superabsorbent in the first and second middle layers
is adjusted such that there is a higher level of superabsorbent in the second
middle layer. The superabsorbent in the first and second middle layers can
be the same or a different superabsorbent.
In one embodiment, the cellulosic fiber for use in the second
absorbent layer 48 is wood pulp. There are certain characteristics of wood
pulp that make it particularly suitable for use. Cellulose in most wood pulps
has a crystalline form known as Cellulose I which can be converted to a form
known as Cellulose II. in the second absorbent layer 48, wood pulp with a
substantial portion of the cellulose as Cellulose II could be used. Similarly,
pulps having an increased fiber curl value are advantageous. Finally, pulps
having reduced levels of hemicellulose are preferred. Means for treating
pulps so as to optimize these characteristics are well known in the art. By
way of example, treating wood pulp with liquid ammonia is known to convert
cellulose to the Cellulose II structure and to increase the fiber curl value.
Flash drying is known to increase the fiber curl value of pulp. Cold caustic
treatment of pulp decreases hemicellulose content, increases fiber curl and
converts cellulose to the Cellulose II form. Thus it could be advantageous

that the cellulosic fibers used to produce the material of this invention
contain at least a portion of cold caustic treated pulp.
A description of the cold caustic extraction process can be found in U.S. patent application Ser. No. 08/370,571, filed on Jan. 18, 1995, pending
which application is a continuation-in-part application of U.S. patent
application Ser. No. 08/184,377, now abandoned filed on Jan. 21, 1994. The
disclosures of both of these applications are incorporated in their entirety
herein by reference.
Briefly, a caustic treatment is typically carried out at a temperature
less than about 60 degree C, but preferably at a temperature less than 50
degree C, and more preferably at a temperature between about 10 degree
C. to 40 degree C. A preferred alkali metal salt solution is a sodium
hydroxide solution newly made up or as a solution by-product in a pulp or
paper mill operation, e.g., hemicaustic white liquor, oxidized white liquor and
the like. Other alkali metal salts such as ammonium hydroxide and
potassium hydroxide and the like can be employed. However, from a cost
standpoint, the preferable salt is sodium hydroxide. The concentration of
alkali metal salts is typically in a range from about 2 to about 25 weight
percent of the solution, and preferably from about 6 to about 18 weight
percent. Pulps for high rate, fast absorbing applications are preferably
treated with alkali metal salt concentrations from about 10 to about 18 weight
percent.
For further details on the structure and the method of construction of
the second absorbent layer 48 the reader is invited to refer to the US patent

5,866,242 granted on February 2, 1999 to Tan et al. The contents of this
document are hereby incorporated by reference.
Main Body-Barrier Layer
Underlying the absorbent system 44 is a barrier layer 50 comprising
liquid-impervious film material so as to prevent liquid that is entrapped in the
absorbent system 44 from egressing the sanitary napkin and staining the
wearer's undergarment. The barrier layer 50 is made preferably of polymeric
film.
The cover layer 42 and the barrier layer 50 are joined along their
marginal portions so as to form an enclosure or flange seal that maintains
the absorbent system 44 captive. The joint may be made by means of
adhesives, heat-bonding, ultrasonic bonding, radio frequency sealing,
mechanical crimping, and the like and combinations thereof. The peripheral
seal line is shown in Figure 1 by the reference numeral 52.
Flaps
The flaps 38 and 40 are preferably made as integral extensions of the
cover layer 42 and the barrier layer 50. These integral extensions are joined to
one another along their marginal seal portions by adhesives, heat-bonding,
ultrasonic bonding, radio frequency sealing, mechanical crimping, and the like
and combinations thereof. Most preferably, such joining is made at the same
time the cover layer 42 and the barrier layer 50 are bonded to one another to
enclose the absorbent system 44. Alternatively, the flaps may include
absorbent material between the cover layer and the barrier layer extensions.

Such absorbent material may be an extension of the first absorbent layer 46,
the second absorbent layer 48 or both.
Adhesive system
Referring to Figures 2 and 3, in order to enhance the stability of the
sanitary napkin, the garment facing surface of the barrier layer is provided
with positioning adhesive material 58, typically hot-melt adhesive material
capable of establishing a temporary bond with the undergarment material. A
suitable material is the composition designated HL-1491 XZP commercially
available from H.B. Fuller Canada, Toronto, Ontario, Canada. The
positioning adhesive 58 may be applied to the garment-facing surface of the
barrier layer 50 in various patterns, including complete adhesive coverage,
parallel longitudinal lines, a line of adhesive following the perimeter of the
structure, transverse lines of adhesive or the like.
Standard release paper 82 (shown only in Figure 3) covers the
positioning adhesive 58 before the napkin is used to prevent the unwanted
adherence of the napkin to itself or foreign objects. The release paper is of
conventional construction (e.g. silicone coated wet-laid Kraft wood pulp) and
suitable papers are available from Tekkote Corporation (Leonia, New Jersey,
USA), and bear the designation FRASER 30#/61629.
The main body of the sanitary napkin is provided with at least one
bending zone and preferably a pattern of bending zones to assist the
sanitary napkin in folding according to a certain three-dimensional profile in use. in this specification, "three-dimensional deformation profile" means a
deformation in the Z direction (vertical direction). Figures 11 and 12 illustrate

examples of such three-dimensional profiles. Figure 11 shows the sanitary
napkin 20 of Figure 1 in cross-section acquiring the "W" pattern where the
central portion of the sanitary napkin 20 is raised to form a central upper
apex while the zones of the sanitary napkin 20 between the central zone and
the longitudinal sides 30, 32 are folded down to form two down apexes. This
folding configuration is considered to reduce the likelihood of leakage by
virtue of the central upper apex that is positioned close to the vaginal
opening of the user, thus it is close to the source of the liquid discharge and
as such can better acquire the liquid.
Figure 12 illustrates the sanitary napkin 20 of Figure 1 in cross-
section acquiring the "M" pattern where the central portion of the sanitary
napkin 20 is lowered to form a central down apex while the zones of the
sanitary napkin 20 between the central zone and the longitudinal sides 30,
32 are folded up to form two upper apexes. This folding configuration is
considered to enhance the comfort potential of the sanitary napkin 20 by
locating the central portion of the sanitary napkin away from the body, thus
reducing contact of the surface of the sanitary napkin with the body of the
user. The centre of the "M" also forms a receptacle accommodating the
labia majora of the user and capable of capturing a fluid discharge
emanating therefrom.
The exemplary sanitary napkin construction depicted in Figure 1,
features a pattern of bending zones having three components, namely a
central bending zone 100 and two linear longitudinally extending preferential
bending zones 102 and 104. The longitudinally extending preferential
bending zones 102 and 104 are located between the central bending zone
100 and the side edges 30, 32 of the sanitary napkin 20.

The sanitary napkin includes an array of oblique preferential bending
lines intersecting each other to create a pattern extending over a major
portion of the longitudinal dimension of the main body. The oblique
preferential bending lines are arcuate and are created on the cover layer and
absorbent system. Under this specific example of implementation, the
preferential bending lines cross one another and form an array of crossing
points. The crossing points are located substantially along the longitudinal
axis of the sanitary napkin and structurally weaken the sanitary napkin at
that location allowing the sanitary napkin to fold preferentially along a
longitudinal axis to form an up apex of a V profile as shown in Figure 13, or a
down apex of an inverted V profile as shown in Figure 14, when subjected to
lateral compression. It is the array of crossing points that forms the
preferential bending zone 100 substantially along the longitudinal center line
of sanitary napkin 20.
Each preferential bending line of the array of bending lines extends
generally along an angle of 45 degrees with respect to the longitudinal axis
of the main body of the sanitary napkin. The pattern is designed such that
each preferential bending line intersects at least two other preferential
bending lines. Also, each preferential bending line extends from one
longitudinal side area of the sanitary napkin to the opposite longitudinal side
area, crossing the imaginary longitudinal axis of the sanitary napkin. A
longitudinal side area is defined as a portion of the sanitary napkin that
extends inwardly from a respective longitudinal side edge 30, 32, the side
edge forming the outer boundary of the side area (the longitudinal side edge
is considered part of the longitudinal side area). Each side area has a width

that is about 25% of the maximal transverse dimension of the main body 22
(excluding the flaps).
In a preferred embodiment, the array of bending lines forms a first
preferential bending zone substantially along the central longitudinal axis of
sanitary napkin 20 and second and third preferential bending zones within
the longitudinal side areas of the sanitary napkin 20. in this preferred
embodiment, the preferential bending zones are formed by the intersections
of the array of bending lines causing the cross-section of the sanitary napkin
20 to acquire an "M" profile where the first preferential bending zone
substantially along the central axis of the sanitary napkin forms a down
apex, and the second and third preferential bending zones within the
longitudinal side areas form up apexes; or a "W" profile where the first
preferential bending zone substantially along the central axis of the sanitary
napkin forms an up apex, and the second and third preferential bending
zones within the longitudinal side areas form down apexes.
Without intent of being bound by a specific theory, it is believed that
the plurality of oblique preferential bending lines contribute to increase the
flexural resistance to lateral compression of the sanitary napkin which has
the effect of stabilising the sanitary napkin against bunching. At the same
time, the oblique preferential bending lines form the central preferential
bending zone at their crossing points.
In a specific example, the spacing between preferential bending lines
is about 2 cm.

In a further embodiment of the sanitary napkin 20 of the invention,
wherein the sanitary napkin has side flaps 38, 40, the second and third
preferential bending zones are formed along the longitudinal side edges of
the sanitary napkin at the junction of the side flaps with the side edge. in this
embodiment, the first absorbent layer preferably has a width that is greater
than the width of the second absorbent layer so that longitudinal side edges
of the first absorbent layer extend beyond longitudinal side edges of the
second absorbent layer. The second and third preferential bending zones
may be formed by an array of preferential bending lines or by the junctions
of the side flaps with the respective longitudinal side edges of the napkin or
by the longitudinal side edges of the first absorbent layer. in cross-section
the sanitary napkin of this embodiment may acquire an "M" profile or a "W"
profile.
In an alternative embodiment, the array of preferential bending lines
are created on the absorbent system only, such as on the first absorbent
layer 46, the second absorbent layer 48 or both, so that the preferential
bending lines are less visible on the sanitary napkin than when the
preferential bending lines are made on the cover layer and absorbent
system.
As discussed earlier, the pattern of bending zones on the sanitary
napkin 20 can assist the sanitary napkin to acquire a three-dimensional
deformation profile. The three-dimensional deformation profile includes
either a "W" or an "M" profile, among other possible profiles. One profile can
be privileged over the other type of deformation profile by controlling on
which main surface (top surface or bottom surface) of the second absorbent
layer the pattern of bending zones is distributed. The embodiment of the

invention shown in Figure 1 is designed to preferentially fold according to the
"W" pattern. When the sanitary napkin 20 is subjected to lateral
compression, it folds up at the longitudinal axis forming a central apex at that
location and also folds down at the two longitudinally extending preferential
bending zones 102 and 104 forming two down apexes.
Figure 7 is a cross-sectional view of the second absorbent layer 48.
The second absorbent layer 48 includes a pattern of bending zones
comprising a central longitudinally extending bending zone 700 formed on
the upper main surface of the second absorbent layer 48 and extending
along the longitudinal axis of the second absorbent layer 48 that coincides
with the longitudinal axis of the sanitary napkin 20. Preferably, the bending
zone 700 extends the full length of the second absorbent layer 48. The
longitudinally extending lateral bending zones 102 and 104 are formed on
the lower main surface of the second absorbent layer 48.
In use, a sanitary napkin 20 with the second absorbent layer shown in Figure 7, when subjected to lateral compression will more easily acquire the
"W" pattern shown in Figure 11.
Figure 8 is a variant of the second absorbent layer 48 shown in Figure
7, where the position of the preferential bending zones has been reversed by
comparison to the embodiment of Figure 7. This provides a structure that
more easily fold according to the "M" pattern shown in Figure 12.
In another alternative embodiment, a single longitudinally extending
continuous bending line extending along the longitudinal axis of the sanitary
napkin can replace the array crossing points. As shown in Figure 9, the

preferential bending zone 700 is materialised by a slit that parts the second
absorbent layer 48 in two separate halves. To control the deformation of the
second absorbent layer, an optional abutment member 900 is placed under
the slit such that the second absorbent layer 48 when subjected to lateral
compression will fold up (inverted V shape) in the centre. The abutment
member 900 can be a strip of synthetic foam material that extends under
both halves of the second absorbent layer 48. This structure favours the
formation of the "W pattern in use. A variant is to make the slit shorter than
the length of the second absorbent layer 48 such that the slit does not part
the second absorbent layer 48 in two. Also, the slit can be replaced by a
series of small perforations behaving as a preferential bending zone.
Figure 10 shows yet another variant of the second absorbent layer 48
that is identical to the example depicted in Figure 8 with the exception of the
lateral longitudinally extending bending zones 102 and 104 formed on the
upper main surface of the second absorbent layer 48. This structure also
favours the formation of the "W pattern in use.
Method of manufacture
The above-described embodiment of the sanitary napkin 20 is
fabricated in a conventional manner in accordance with conventional
techniques. Specifically, a laminate structure, sometimes referred to in the
art as a web, is created. This laminate structure comprises an expanse of
the materials from which the napkin will be created. I.e. the laminate
structure comprises the following layers of material in a top-to-bottom order:
an expanse of cover layer material; an expanse of first absorbent layer
material; an expanse of second absorbent layer material (manufactured as

described above); and finally an expanse of barrier layer material. Some of
the materials are necessarily not continuous within the laminate structure,
and where such is the case, they are positioned precisely, one with respect
to another, in the relationship they will occupy in the final products. The
cover layer material and the barrier layer material are then bonded together
by applying pressure in the appropriate positions, and what will become the
peripheral seal is created. The seal may also be made by means of heat-
bonding, ultrasonic bonding, radio frequency sealing, mechanical crimping,
and the like and combinations thereof. The sealed structure is then severed
by conventional means (i.e. die-cutting, fluid-jet cutting, or by laser) from the
web to create a discrete article.
The preferential bending zones are created preferably by embossing.
The choice of embossing is not critical since the same result may be
obtained by other methods also such as slitting, perforating or other
techniques known to those skilled in the art. If the embossing operation is
chosen to create the preferential bending zones, the sanitary napkin is
passed between a pair of rolls, one of the rolls including projections
according to the pattern of embossing desired. The projections locally
compress the material of the sanitary napkin, which can be either a
combination of the cover layer and the absorbent system or the absorbent
system alone, thereby compacting it. The degree of pressure applied during
the embossing operation can vary depending upon the type of material
embossed and the physical integrity of the material embossed, among
others. It is within the reach of a person skilled in the art to find the optimal
process conditions in accordance with the specific application. in general,
the embossing pressure should be selected to sufficiently density the
material locally so as to create the preferential bending zones and at the

same time not to be too high so as to sever the material. Heating the
embossing rolls has been found beneficial. Also, ultrasonic embossing may
be used for forming the preferential bending zones.
It is preferred to emboss the entire sanitary napkin as the embossing
also holds the various layers of the sanitary napkin together and reduces the
likelihood of the cover layer or the barrier layer gapping or coming loose
when the sanitary napkin is bent.
The positioning adhesive material is then applied to the barrier layer in the appropriate positions, and release paper is applied to cover the
positioning adhesive. Alternatively, the positioning adhesive, or the
positioning adhesive and the release paper may be applied to the web
before the individual articles are severed therefrom.
As indicated earlier, the sanitary napkin 20 has a thickness of less
than about 4 mm or less. The apparatus required to measure the thickness
of the sanitary napkin is a footed dial (thickness) gauge with stand, available
from Ames, with a 2" diameter foot and a readout accurate to 0.001". A
digital type apparatus is preferred. If the sanitary napkin sample is
individually folded and wrapped, the sample is unwrapped and carefully
flattened by hand. The release paper is removed from the sample and it is
repositioned back gently across the positioning adhesive lines so as not to
compress the sample, ensuring that the release paper lies flat across the
sample. Flaps (if any) are not considered when taking the thickness reading
of the sample.

The foot of the gauge is raised and the sample is placed on the anvil
such that the foot of the gauge is approximately centered to the sample (or in the location of interest on the sample of interest). When lowering the foot,
care is taken to avoid allowing the foot to "drop" or that undue force is not
applied. The read out is allowed to stabilize for approximately 5 seconds.
The thickness reading is then taken.
The flexural resistance of the sanitary napkin is preferably in the
range from about 400g to about 800 g. The flexural resistance of a sanitary
napkin is measured by peak bending stiffness. Peak bending stiffness is
determined by a test that is modeled after the ASTM D 4032-82 CIRCULAR
BEND PROCEDURE, the procedure being considerably modified and
performed as follows. The CIRCULAR BEND PROCEDURE is a
simultaneous multi-directional deformation of a material in which one face of
a specimen becomes concave and the other face becomes convex. The
CIRCULAR BEND PROCEDURE gives a force value related to flexural
resistance, simultaneously averaging stiffness in all directions.
The apparatus necessary for the CIRCULAR BEND PROCEDURE is
a modified Circular Bend Stiffness Tester, having the following parts:
1. A smooth-polished steel plate platform which is 102.0 mm by 102.0 by
6.35 mm having an 18.75 mm diameter orifice. The lap edge of the orifice
should be at a 45 degree angle to a depth of 4.75 mm;
2. A plunger having an overall length of 72.2 mm, a diameter of 6.25
mm, a ball nose having a radius of 2.97 mm and a needle-point extending
0.88 mm therefrom having a 0.33 mm base diameter and a point having a

radius of less than 0.5 mm, the plunger being mounted concentric with the
orifice and having equal clearance on all sides. Note that the needle-point is
merely to prevent lateral movement of the test specimen during testing.
Therefore, if the needle-point significantly adversely affects the test
specimen (for example, punctures an inflatable structure), than the needle-
point should not be used. The bottom of the plunger should be set well
above the top of the orifice plate. From this position, the downward stroke of
the ball nose is to the exact bottom of the plate orifice;
3. A force-measurement gauge and more specifically an Instron inverted
compression load cell. The load cell has a load range of from about 0.0 to
about 2000.0 g;
4. An actuator and more specifically the Instron Model No. 1122 having
an inverted compression load cell. The Instron 1122 is made by the Instron
Engineering Corporation, Canton, Mass.
In order to perform the procedure for this test, as explained below,
five representative sanitary napkins are necessary. From one of the five
napkins to be tested, some number "Y" of 37.5 mm by 37.5 mm test
specimens are cut. Specimens having portions in which a cover layer is
joined directly to a barrier layer or which are a laminate of a cover layer, and
a barrier layer without any component of the absorbent system, should not
be tested. This test is more concerned with the overall flexibility of the
sanitary napkin and not merely the peripheral portions thereof and, therefore,
the flexibility of the present invention is more concerned with the flexibility of
the absorbent portions of the sanitary napkin.

The test specimens should not be folded or bent by the test person,
and the handling of specimens must be kept to a minimum and to the edges
to avoid affecting flexural-resistance properties. From the four remaining
sanitary napkins, an equal number "Y" of 37.5 mm by 37.5 mm specimens,
identical to the specimens cut from the first napkin, are cut. Thus, the test
person should have "Y" number of sets of five identical specimens.
The procedure for the CIRCULAR BEND PROCEDURE is as follows.
The specimens are conditioned by leaving them in a room that is 21 degree
Celsius plus or minus 1 degree Celsius and 50% plus or minus 2% relative
humidity for a period of two hours. The test plate is leveled. The plunger
speed is set at 50.0 cm per minute per full stroke length. A specimen is
centered on the orifice platform below the plunger such that the cover layer
42 of the specimen is facing the plunger and the barrier layer 50 of the
specimen is facing the platform. The indicator zero is checked and adjusted,
if necessary. The plunger is actuated. Touching the specimen during the
testing should be avoided. The maximum force reading to the nearest gram
is recorded. The above steps are repeated until all five of the identical
specimens have been tested.
CALCULATIONS
The peak bending stiffness for each specimen is the maximum force
reading for that specimen. Remember that "Y" number of sets of five
identical specimens were cut. Each set of five identical specimens is tested
and the five values received for that set are averaged. Thus, the test person
now has an average value for each of the "Y" sets tested. The flexural

resistance for a sanitary napkin is the greatest of these average peak
bending stiffnesses.
Applications of the product and methods of the present invention for
sanitary and other health-care uses can be accomplished by any sanitary
protection, incontinence, medical and absorbent methods and techniques as
are presently or prospectively known to those skilled in the art. Thus, it is
intended that the present application cover the modifications and variations
of this invention provided that they come within the scope of the appended
claims and their equivalents.

WE CLAIM;
1. A sanitary napkin adapted to be worn in a crotch portion of an undergarment,
said sanitary napkin comprising:
a) a fluid-pervious cover layer (42);
b) an absorbent system (44) under said cover layer (42) said absorbent
system (44) having a central width of at least 64 mm;
c) a liquid-impervious barrier layer (50) under said absorbent system(44);
d) said sanitary napkin being characterised by a thickness less than about
5mm;
e) said sanitary napkin being characterised by a flexural resistance of not
less than about 400 g;
f) said sanitary napkin having a main body (20) with a longitudinal axis (34)
and two opposite longitudinal side areas (30,32) said sanitary napkin
including a preferential bending line extending obliquely in relation to said
longitudinal axis on said main body, said preferential bending line
extending from one longitudinal side area of the sanitary napkin to an
opposite longitudinal side area, crossing the longitudinal axis of the
sanitary napkin.

2. A sanitary napkin as defined in claim 1, wherein said bending line is formed by
embossing said absorbent system.
3. A sanitary napkin as defined in claim 2, wherein said sanitary napkin includes a
plurality of preferential bending lines crossing one another and defining an array
of crossing points thereby forming at least one preferential bending zone allowing
said sanitary napkin to fold at said preferential bending zone in response to
lateral compression applied to said napkin and permitting said napkin to acquire
a three-dimensional deformation profile.

4. A sanitary napkin as defined in claim 3. wherein the crossing points in the array
or crossing points extend along the longitudinal axis and facilitate folding or said
sanitary napkin at a location along the longitudinal axis.
5. A sanitary napkin as defined in claim 4, wherein said preferential bending zone is
a central preferential bending zone, said absorbent system further including a
pair of ilnear preferential bending zones extending between said central
preferential bending zone and respective side edges of said sanitary napkin.
6. A sanitary napkin as defined in claim 1, wherein said three dimensional
deformation profile is a W profile.
7. A sanitary napkin as defined in claim 1, wherein said three dimensional
deformation profile is a M profile.
8. A sanitary napkin as defined in claim 1, wherein said sanitary napkin includes a
pair of longitudinally extending side edges, said absorbent system comprises a
top surface and a bottom surface and includes:
two preferential being zones extending along said longitudinal axis and being
adjacent the side edges of said napkin on said top surface of said absorbent
system; and
a preferential being zone on the bottom surface of said absorbent system
extending along said longitudinal axis, between the two preferential bending
zones adjacent the side edges of said napkin.

9. A sanitary napkin as denned in claim 1, wherein said sanitary napkin includes a
pair of longitudinally extending side edges, said absorbent system comprises a
top surface and a bottom surface and includes:
two preferential bending zones extending along said longitudinal axis and being
adjacent the side edges of said napkin on said bottom surface of said absorbent
system; and
a preferential bending zone on the top surface of said absorbent system
extending along said longitudinal axis, between the two preferential bending
zones adjacent the side edges of said napkin.
10. A sanitary napkin as defined in claim 6, wherein one of said preferential bending
zones extending is formed by a process selected from the group consisting of
perforating, slitting, cutting and embossing.
11. A sanitary napkin as defined in claim 6, wherein the two preferential bending
zones extending longitudinally near the side edges of said napkin are arcuate.
12. A sanitary napkin as defined in claim 6, wherein said preferential bending zone
extending longitudinally in the central portion of said napkin is comprised of a
continuous line of embossing.
13. A sanitary napkin as defined in claim 6, comprising an elongated strip of material
adjacent one of the top surface or bottom surface of said absorbent system and
extending along said longitudinal axis, said elongated strip of material inducing
said absorbent system to fold about the preferential bending zone between the
two preferential bending zones adjacent the side edges of said napkin, in a
direction away from said strip.

14. A sanitary napkin as defined in claim 1. wherein said absorbent system includes
superabsorbent material.

15. A sanitary napkin as defined in claim 12, wherein said absorbent system includes
a blend of cellulosic fibers and superabsorberrt material.
16. A sanitary napkin as defined in claim 13, wherein said absorbent system includes
an absorbent layer having a basis weight of from about 100 g/m2 to about 700
g/m2 which has been air-laid as a bottom stratum of pulp, a middle stratum cf
pulp and superabsorberrt polymer disposed in amongst the pulp, and a top
stratum containing at least some pulp.
17. A sanitary napkin as defined in claim 14, wherein said absorbent system includes
a plurality of absorbent layers in a superposed condition.
18. A sanitary napkin as defined in claim 1, wherein said sanitary napkin includes a
fastener for retaining said sanitary napkin on an undergarment of a wearer.
19. A sanitary napkin as defined in claim 16, wherein said fastener includes a flap.



ABSTRACT


TITLE: A SANITARY NAPKIN ADAPTED TO BE WORN IN A
CROTCH PORTION OF AN UNDERGARMENT
A sanitary napkin adapted to be worn in a crotch portion of an undergarment,
said sanitary napkin comprising:
a) a fluid-pervious cover layer (42);
b) an absorbent system (44) under said cover layer (42) said absorbent system
(44) having a central width of at least 64 mm;
c) a liquid-impervious barrier layer (50) under said absorbent system(44);
d) said sanitary napkin being characterised by a thickness less than about 5mm;
e) said sanitary napkin being characterised by a flexural resistance of not less
than about 400 g;
f) said sanitary napkin having a main body (20) with a longitudinal axis (34) and
two opposite longitudinal side areas (30,32) said sanitary napkin including a
preferential bending line extending obliquely in relation to said longitudinal
axis on said main body, said preferential bending line extending from one
longitudinal side area of the sanitary napkin to an opposite longitudinal side
area, crossing the longitudinal axis of the sanitary napkin.

Documents:

462-cal-2000-abstract.pdf

462-CAL-2000-CANCELLED PAGES.pdf

462-cal-2000-claims.pdf

462-CAL-2000-CORRESPONDENCE-1.1.pdf

462-cal-2000-correspondence.pdf

462-cal-2000-description (complete).pdf

462-CAL-2000-EXAMINATION REPORT-1.1.pdf

462-cal-2000-examination report.pdf

462-cal-2000-form 1.pdf

462-CAL-2000-FORM 18-1.1.pdf

462-cal-2000-form 18.pdf

462-cal-2000-form 2.pdf

462-CAL-2000-FORM 26-1.1.pdf

462-cal-2000-form 26.pdf

462-cal-2000-form 3.pdf

462-cal-2000-form 5.pdf

462-CAL-2000-GRANTED-ABSTRACT.pdf

462-CAL-2000-GRANTED-CLAIMS.pdf

462-CAL-2000-GRANTED-DESCRIPTION (COMPLETE).pdf

462-CAL-2000-GRANTED-DRAWINGS.pdf

462-CAL-2000-GRANTED-FORM 1.pdf

462-CAL-2000-GRANTED-FORM 2.pdf

462-CAL-2000-GRANTED-FORM 3.pdf

462-CAL-2000-GRANTED-FORM 5.pdf

462-CAL-2000-GRANTED-SPECIFICATION-COMPLETE.pdf

462-CAL-2000-OTHERS.pdf

462-CAL-2000-PETITION UNDER RULE 137.pdf

462-CAL-2000-REPLY TO EXAMINATION REPORT-1.1.pdf

462-cal-2000-reply to examination report.pdf

462-cal-2000-specification.pdf

462-CAL-2000-TRANSLATED COPY OF PRIORITY DOCUMENT-1.1.pdf

462-cal-2000-translated copy of priority document.pdf


Patent Number 261038
Indian Patent Application Number 462/CAL/2000
PG Journal Number 23/2014
Publication Date 06-Jun-2014
Grant Date 30-May-2014
Date of Filing 16-Aug-2000
Name of Patentee JOHNSON & JOHNSON INC.
Applicant Address 7101 NORTE DAME STREET, EAST, MONTREAL, QUEBEC, CANADA H1N 2G4
Inventors:
# Inventor's Name Inventor's Address
1 BRISEBOIS, HENRI 2129 RUE FLORENT, LACHENAIE, QUEBEDC, J6W 3T8
2 CANUEL LOUIS 79 JASMIN, REPENTIGNY, QUEBEC, J6A 5V6
3 LARIVIERE CHRISTIANE 1710 BOURBONNIERE, APT.5, MONTREAL, QUEBEC H1W 3N4
4 MURJI ZULFIKAR 146, RUE FRANCOIS, NO.205, VERDUN QUEBEC H3E 1G3
PCT International Classification Number A61F 13/15
PCT International Application Number N/A
PCT International Filing date
PCT Conventions:
# PCT Application Number Date of Convention Priority Country
1 09/375343 1999-08-16 U.S.A.
2 09/477244 2000-01-04 U.S.A.